Izinkinga ezijwayelekile zemishini ye-rotary kiln

Dec 09, 2021

Shiya umlayezo

1. Run ukudla okuluhlaza

Ngenani elithile lokudla okuluhlaza okuluhlaza, inani lamalahle asetshenzisiwe lincane, Ukulawulwa kokusetshenziswa kokushisa kuphansi, futhi izinga lokushisa le-calt alwanele akwanele; Ukwakheka kwendandatho noma inani elikhulu lesikhumba se-Kiln Collapses, futhi ivolumu engenayo engazelelwe yanda, futhi opharetha akazi noma banake noma banake. Inani lamalahle nejubane le-kiln alilungiswa ngesikhathi noma ukwahlulela akulungile; Ukusetshenziswa kwamalahle kwe-calciner kuncane kakhulu, inani lokukhomba lezinto ezingavuthiwe ku-kiln liphansi, i-kiln isebenzisa inani elikhulu lamalahle kepha umoya omncane we-kiln awumuhle, futhi izinga lokushisa lendawo elivuthayo alikwazi ukukhuliswa. Ukukhishwa kwe-rotary kiln kusebenza ebangeni eliphansi, elibangela ukwenzeka kaningi kokuwa ngokwezinto ezibonakalayo ohlelweni lwe-PreHoter.

2

Ukuvulwa kwe-valve fan of the offer of the cooler kukhulu kakhulu; I-Clinker Cooding Fan yehluleka noma ungqimba lwezinto ezibonakalayo lukhulu kakhulu futhi ukumelana kukhulu kakhulu, kuphumela ekwehleni kwevolumu yomoya opholile; Umsila we-kiln umsila we-ash kanye nomgodi olandelayo uvulwe kungazelelwe, futhi ukuncela kwesistimu kuncishisiwe.

3. Izinga lokushisa lomsila we-kiln kanye nohlelo lokukhohlisa luphezulu kakhulu

Ukungena komoya kwemishini ye-rotary kiln akukuhle; Ukuhlinzekwa kwezinto zokwakha akulungile noma akunakulingani; Izinga lokushisa lesistimu lenyuka ngenxa yokuvinjelwa kwesiphepho; Izinga lokushisa lendawo evuthayo liphansi kakhulu, futhi amalahle adonswayo ashisiwe.

4. Amazinga okushisa egesi wokuphelelwa yipholi aphezulu kakhulu

Ipuleti le-grate lama-run ahlanganisiwe ngokushesha okukhulu, futhi i-clinker ingena phakathi noma ngemuva kwendawo epholile ngaphandle kokupholisa okwanele; I-Clinker Cooding Air Volume anganele, futhi izinga lokushisa le-clinker liphuma endaweni epholile, kanti izinga lokushisa legesi eliphelelwe yilona ngokwemvelo likhuphuka.

I-5. Izinga lokushisa lendawo yokudubula liphezulu kakhulu

Izinto ezingenayo zincane futhi inani lamalahle asetshenzisiwe alincishiwe ngesikhathi; Ukugeleza komoya ku-burner kukhulu kakhulu, okubangela ilangabi lifushane kakhulu futhi indawo ephezulu yokushisa igxile kakhulu; Amazinga okushisa amoyeni wesibili aphezulu kakhulu, inhloko yelangabi emnyama imfushane, futhi iphuzu lomlilo lidluliselwe phambili.

6. Ukushisa komoya kwesibili kuphansi kakhulu

I-nozzle inwebeka ngaphakathi, ilangabi lide, futhi kukhona ubude obuthile bendawo yokupholisa ku-kiln; IVolumu Yomoya ye-High - Ingcindezelo Fan egumbini lokuqala le-Colover likhulu kakhulu; I-Clinker ku-grate isatshalaliswa ngokungalingani, futhi umoya opholile ufushane -, ongenawo umphumela wokupholisa.

7

Kusetshenziswa amalahle amaningi kakhulu futhi izinga lokushisa lokudubula liphezulu kakhulu; Ukudla okuluhlaza akusona ama-homogenized, ukwakheka kwamakhemikhali kushintshashintsha kakhulu, noma ubuwula bokudla obuluhlaza buhle kakhulu, okwenza lokho kube lula kakhulu ukubango; Lapho uthuli lwe-kiln lungezwe ngqo kwi-kiln, isilinganiso sokuxuba esisheshayo sikhulu kakhulu.

8. I-Kiln Ring formation

Ukushisa komoya wesibili kuphezulu isikhathi eside, ijubane lokuhlanza amalahle engcolisa lishesha kakhulu, futhi ilangabi ligxile kakhulu; Izinga lokushisa lendawo evuthayo liphezulu kakhulu, futhi lokho kudilizwa; Izinhlayiya ze-Clinker zihamba kahle kakhulu futhi i-powder inkulu kakhulu. Ukuvulwa kwe-valve kwe-high - Ingcindezelo fan egumbini lokuqala le-cooler enkulu kakhulu, inani elikhulu lempuphu libuyiselwa kwi-rotary kiln.


Thumela ukuPhenya